Lubriplate X-Heavy G.S. Lithium Based Grease For Open Gearing

Category Fluid , Lubricant , Lithium Gellant
Manufacturer Lubriplate Lubricants
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubriplate X-Heavy G.S. Lithium Based Grease For Open Gearing.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lithium-based open gear grease made for all types of open gears. Available in 4 formulas for a variety of conditions and temperatures. Gear Shield Extra Heavy is for adverse conditions.Applications: Open gears, adverse conditions. Excellent for fifth wheel applications.Gear Shield X-Heavy is available in Aerosol, Caulk Type Cartridges, Cans, Pails, 1/4 Drums & Drums.Information provided by Lubriplate
Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 2000 SUS
2000 SUS
Kinematic Viscosity at 40°C (104°F) 432 cSt
432 cSt
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 235
235
Unknown Amount of Work
Penetration P(60), 1/10 mm 260
260
Unknown Amount of Work
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -6.67 °C
20.0 °F
Approx. Cold test
Dropping Point 188 °C
370 °F
ASTM Test
Descriptive Properties Value Comments
Antiwear (AW)/ Extreme Pressure (EP) AW
NLGI Grade 2.5
Rust/Oxidative Additives YES
Water Resistant YES