Thermal Properties | Metric | English | Comments |
---|---|---|---|
Dropping Point | 188 °C | 370 °F | ASTM Test |
Lubriplate X-Heavy G.S. Lithium Based Grease For Open Gearing Lithium-based open gear grease made for all types of open gears. Available in 4 formulas for a variety of conditions and temperatures. Gear Shield Extra Heavy is for adverse conditions.Applications:.. |
|||
Dropping Point | 188 °C | 370 °F | ASTM D2265 |
ExxonMobil Greasrex K-218 Greasrex K-218 is an NLGI grade 2 product designed for the post tension construction industry. It has controlled oil bleed to prevent oil separation on tendon manufacture. It has exceptional corrosi.. |
|||
Dropping Point | 188 °C | 370 °F | |
ChevronTexaco Dura-Lith® NLGI 2 Grease EP FeaturesChevron Dura-Lith Greases EP are multipurpose extreme pressure greases.They are manufactured using selected highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thic.. |
|||
Dropping Point | 188 °C | 370 °F | |
ChevronTexaco Marfak® Multipurpose NLGI Grade 2 Texaco Marfak Multipurpose delivers value through:Good water resistance — Provides lubrication in the presence of water.Good corrosion protection — Inhibited to protect gear and bearing surfaces.G.. |
|||
Dropping Point | 188 °C | 370 °F | |
ChevronTexaco Multifak® AFB NLGI Grade 2 Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.Notes:Minimum operating temperature is the lowest tempe.. |
|||
Dropping Point | 188 °C | 370 °F | |
ChevronTexaco Multifak® EP NLGI Grade 2 Texaco Multifak EP greases deliver value through:Good water resistance — Strong resistance to wash out of bearings.Good rust and corrosion protection, even in wet conditions.Extreme pressure protec.. |
|||
Dropping Point | 188 °C | 370 °F | |
ChevronTexaco Threadtex® Texaco Threadtex delivers value through:High antiweld protection — Drill collars "break" easily. No galled or broken threads.Excellent lubrication in the presence of water, drilling muds, etc. Prov.. |
|||
Dropping Point | 188 °C | 370 °F | ASTM D2265 |
ExxonMobil Greasrex K-218 Greasrex K-218 is an NLGI grade 2 product designed for the post tension construction industry. It has controlled oil bleed to prevent oil separation on tendon manufacture. It has exceptional corrosi.. |