Thermal Properties Metric English Comments
Dropping Point 188 °C
370 °F
ASTM Test
Lubriplate X-Heavy G.S. Lithium Based Grease For Open Gearing
Lithium-based open gear grease made for all types of open gears. Available in 4 formulas for a variety of conditions and temperatures. Gear Shield Extra Heavy is for adverse conditions.Applications:..
Dropping Point 188 °C
370 °F
ASTM D2265
ExxonMobil Greasrex K-218
Greasrex K-218 is an NLGI grade 2 product designed for the post tension construction industry. It has controlled oil bleed to prevent oil separation on tendon manufacture. It has exceptional corrosi..
Dropping Point 188 °C
370 °F
ChevronTexaco Dura-Lith® NLGI 2 Grease EP
FeaturesChevron Dura-Lith Greases EP are multipurpose extreme pressure greases.They are manufactured using selected highly refined medium viscosity index base oils, a lithium 12-hydroxystearate thic..
Dropping Point 188 °C
370 °F
ChevronTexaco Marfak® Multipurpose NLGI Grade 2
Texaco Marfak Multipurpose delivers value through:Good water resistance — Provides lubrication in the presence of water.Good corrosion protection — Inhibited to protect gear and bearing surfaces.G..
Dropping Point 188 °C
370 °F
ChevronTexaco Multifak® AFB NLGI Grade 2
Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.Notes:Minimum operating temperature is the lowest tempe..
Dropping Point 188 °C
370 °F
ChevronTexaco Multifak® EP NLGI Grade 2
Texaco Multifak EP greases deliver value through:Good water resistance — Strong resistance to wash out of bearings.Good rust and corrosion protection, even in wet conditions.Extreme pressure protec..
Dropping Point 188 °C
370 °F
ChevronTexaco Threadtex®
Texaco Threadtex delivers value through:High antiweld protection — Drill collars "break" easily. No galled or broken threads.Excellent lubrication in the presence of water, drilling muds, etc. Prov..
Dropping Point 188 °C
370 °F
ASTM D2265
ExxonMobil Greasrex K-218
Greasrex K-218 is an NLGI grade 2 product designed for the post tension construction industry. It has controlled oil bleed to prevent oil separation on tendon manufacture. It has exceptional corrosi..