Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Advanced Materials PEARLCOAT® 162K Thermoplastic Polyurethane Elastomer

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer Lubrizol Advanced Materials Manufacturing S. S.L. (Former Merquinsa)
Trade Name Pearlcoat®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials PEARLCOAT® 162K Thermoplastic Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PEARLCOAT® 162K is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and very good hydrolysis resistance. PEARLCOAT® 162K is used in melt coatings on textile substrates, for end-uses in industrial coatings (for life-jackets, etc.) obtained by extrusion and calendaring. PEARLCOAT® 162K is used for obtaining extruded films and fabric coatings.All information provided by Merquinsa
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
Melt Flow 10 g/10 min

@Load 21.6 kg
10 g/10 min

@Load 47.6 lb
Mechanical Properties Metric English Comments
Hardness, Shore A 82
82
ASTM D2240
Tensile Strength, Yield 30.05 MPa
4359 psi
ASTM D412
Elongation at Break 550 %
550 %
ASTM D412
100% Modulus 0.00501 GPa
0.727 ksi
ASTM D412
300% Modulus 0.01002 GPa
1.453 ksi
ASTM D412
Abrasion 25
25
loss (mm³); DIN 53.516
Thermal Properties Metric English Comments
Melting Point 143 - 154 °C
290 - 310 °F
MQSA 111
Glass Transition Temp, Tg -42.2 °C
-44.0 °F
DSC, 10ºC/min; DIN 51.007
Processing Properties Metric English Comments
Zone 1 160 - 168 °C
320 - 335 °F
Zone 2 168 - 179 °C
335 - 355 °F
Zone 3 179 - 191 °C
355 - 375 °F
Zone 4 185 - 193 °C
365 - 380 °F
Die Temperature 185 - 193 °C
365 - 380 °F