Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 143 - 154 °C | 290 - 310 °F | MQSA 111 |
Lubrizol Advanced Materials PEARLCOAT® 162K Thermoplastic Polyurethane Elastomer PEARLCOAT® 162K is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and very good hydrolysis resistance. PE.. |
|||
Melting Point | 138 - 154 °C | 280 - 310 °F | |
DayGlo ZQ Pigments ZQ-18 Signal Green DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar.. |
|||
Melting Point | 138 - 154 °C | 280 - 310 °F | |
DayGlo ZQ Pigments ZQ-19 Horizon Blue DAY-GLO ZQ-Pigments are an improved version of DAY-GLO Z-Pigments. They offer lower mold plateout, increased plastic compatibility, are mostly stronger, require processing temperatures, and have lar.. |