Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 160 °C | 320 °F | |
DuPont Nucrel® 2906 Ethylene-Methacrylic Acid Copolymer Resin
(discontinued **) Nucrel® 2906 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for.. |
|||
Zone 1 | 160 °C | 320 °F | |
DuPont Nucrel® 2940 Ethylene-Methacrylic Acid Copolymer Resin
(discontinued **) Nucrel® 2940is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Zone 1 | 160 °C | 320 °F | |
Termopol Termoton® K2GA3060A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
Zone 1 | 160 °C | 320 °F | |
Termopol Termoton® K2GA4065A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
Zone 1 | 160 °C | 320 °F | |
Termopol Termoton® K2GA5080A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
Zone 1 | 160 °C | 320 °F | |
Termopol Termoton® K4GA4055A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
Zone 1 | 160 °C | 320 °F | |
Termopol Termoton® K4GA4070A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
Zone 1 | 160 - 180 °C | 320 - 356 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 3140D Ester Type TPE Description: Injection Molding, TPC-ET, Specialty, Low Melting Temperature, Low ModulusApplication: Masterbatch Carrier, Cable Compound BaseCAS: 37282-12-5Information provided by LG Chemical |
|||
Zone 1 | 160 - 175 °C | 320 - 347 °F | Extrusion Molding |
Kolon ELLAS K-296AB Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjection: Pneumatic tube, film/sheet, cableTransparent HoseIndustry Parts Information provided by API-Kolon. |
|||
Zone 1 | 160 - 175 °C | 320 - 347 °F | Injection Molding |
Kolon ELLAS K-470A Ester Based Thermoplastic Polyurethane ApplicationsInjectionIndustry PartsParts for Automobile/Mobile phoneABS Compound |
|||
Zone 1 | 160 - 175 °C | 320 - 347 °F | Injection Molding |
Kolon ELLAS K-590A Caprolactone Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionDust SealOil Seal Information provided by API-Kolon. |
|||
Zone 1 | 160 - 175 °C | 320 - 347 °F | Injection Molding |
Kolon ELLAS K-596A Caprolactone Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionDust SealOil Seal Information provided by API-Kolon. |
|||
Zone 1 | 160 - 175 °C | 320 - 347 °F | Extrusion Molding |
Kolon ELLAS K-792A Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionFlexible HoseIndustry Parts Information provided by API-Kolon. |
|||
Zone 1 | 160 - 175 °C | 320 - 347 °F | Extrusion Molding |
Kolon ELLAS K-793AB Ester Based Thermoplastic Polyurethane ApplicationsFilm/SeatBlown filmIndustry Parts Information provided by API-Kolon. |
|||
Zone 1 | 160 - 175 °C | 320 - 347 °F | Injection Molding |
Kolon ELLAS K-796A Ester Based Thermoplastic Polyurethane ApplicationsExtrusionInjectionPneumatic HoseTransparent HoseIndustry Parts Information provided by API-Kolon. |
|||
Zone 1 | 160 - 170 °C | 320 - 338 °F | |
Silon Taborex TA 1109 MD Chemically-Crosslinkable MDPE Compound TABOREX TA 1110 MD is a crosslinkable compound made by a Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOP.. |
|||
Zone 1 | 160 - 170 °C | 320 - 338 °F | |
Silon Taborex TA 1131 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1131 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Zone 1 | 160 - 170 °C | 320 - 338 °F | |
Silon Taborex TA 1132 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1132 HD is a crosslinkable compound made of Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Zone 1 | 160 - 170 °C | 320 - 338 °F | |
Silon Taborex TA 1133 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1133 HD is a crosslinkable compound made of Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Zone 1 | 160 °C | 320 °F | |
Borealis Borcell™ HE4873 High Density Polyethylene Borcell™ HE4873 is a fully formulated compound for physical foamed data cable insulation. Borcell™ HE4873 is a high-density polyethylene compound containing blowing agent for the production of foa.. |
|||
Zone 1 | 160 °C | 320 °F | Extrusion |
Lubrizol Estane® ZHF 95AT3 Thermoplastic Polyurethane, Flame Retardant Type: Estane® ZHF 95AT3 TPU is a zero halogen flame retardant polyether based thermoplastic polyurethane compound.Features: Outstanding flame retardant properties, especially suited for tray cables.. |
|||
Zone 1 | 160 °C | 320 °F | |
Borealis Casico™ FR6082 Reduced Fire Hazard Jacketing Compound Casico™ FR6082 is a thermoplastic, reduced fire hazard, zero halogen black jacketing compound combined with high mechanical strength, toughness and excellent extrusion properties. It is based on th.. |
|||
Zone 1 | 160 °C | 320 °F | |
DuPont Nucrel® 699 Ethylene-Methacrylic Acid Copolymer Resin Nucrel® 599 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Zone 1 | 160 °C | 320 °F | |
DuPont Nucrel® 925 Ethylene-Methacrylic Acid Copolymer Resin Nucrel® 925 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for .. |
|||
Zone 1 | 160 - 170 °C | 320 - 338 °F | |
Eurostar Starflam MX06101 PP, Flame Retardant, Injection Molding Starflam MX06101 is an Unfilled, Halogen Free Flame Retardant Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 160 - 180 °C | 320 - 356 °F | |
Arkema Group OREVAC® 18365-S Grafted Maleic Anhydride Polyethylene OREVAC 18365-S is a grafted maleic anhydride polyethylene used in the manufacturing of multilayer oxygen barrier tube. OREVAC 18365-S is mainly used in multi-layer tube to have good adhesion between.. |
|||
Zone 1 | 160 °C | 320 °F | |
AdvanSource Biomaterials ChronoFlex® C 80A Biodurable Medical Grade Polyurethane ChronoFlex® C is a family of premium polycarbonate aromatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® C medical-grade elastome.. |
|||
Zone 1 | 160 °C | 320 °F | Extrusion |
Alliance Polymers Zythane™ 5060A Thermoplastic Polyurethane Elastomer Zythane™ 5060A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Zone 1 | 160 °C | 320 °F | |
Termopol Termoton® K2GA2060A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |