Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Estane® ALR E77A-V Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Estane® ALR E77A-V Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type: Estane® ALR E77A-V is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Linear Mold Shrinkage 0.0080 - 0.012 cm/cm
0.0080 - 0.012 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 77
77
ASTM D2240
Tensile Strength, Ultimate 42.7 MPa
6200 psi
ASTM D412
Elongation at Break 550 %
550 %
ASTM D412
100% Modulus 0.00414 GPa
0.600 ksi
ASTM D412
200% Modulus 0.00621 GPa
0.900 ksi
ASTM D412
300% Modulus 0.00965 GPa
1.40 ksi
ASTM D412
Flexural Modulus 0.0159 GPa
2.30 ksi
ASTM D790