Material Notes:
Type: Estane® S190A is a Shore 92A, polyester based thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: AsiaInformation Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 92
92
ASTM D2240
Hardness, Shore D 48
48
ASTM D2240
Tensile Strength, Ultimate 49.0 MPa
7110 psi
ASTM D412
Tensile Strength, Yield 9.32 MPa
1350 psi
at 100% elongation; ASTM D412
18.6 MPa
2700 psi
at 300% elongation; ASTM D412
Elongation at Break 650 %
650 %
ASTM D412
Tear Strength 137 kN/m
784 pli
Die C; ASTM D624
Abrasion 30
30
mm<sup>3</sup> loss; ISO 4649
Compression Set 15 %

@Temperature 23.0 °C,
Time 79200 sec
15 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
40 %

@Temperature 70.0 °C,
Time 79200 sec
40 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395
Thermal Properties Metric English Comments
Vicat Softening Point 110 °C
230 °F
ASTM D1525
Processing Properties Metric English Comments
Feed Temperature 185 - 195 °C
365 - 383 °F
Nozzle Temperature 190 - 205 °C
374 - 401 °F
Mold Temperature 10.0 - 40.0 °C
50.0 - 104 °F
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Dry Time 4.00 - 5.00 hour
4.00 - 5.00 hour
Injection Pressure 8.27 - 13.8 MPa
1200 - 2000 psi
Hold Pressure 8.27 - 12.4 MPa
1200 - 1800 psi
Back Pressure 0.207 - 0.552 MPa
30.0 - 80.0 psi
Cycle Time - Injection 25 - 35 sec
25 - 35 sec
Screw Speed 180 - 220 rpm
180 - 220 rpm
Descriptive Properties Value Comments
Injection time (s) 12-18
Metering Zone 185-200°C