Lubrizol Stat-Rite® S-102 Static Control Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Lubrizol (former Noveon)
Trade Name Stat-Rite®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Stat-Rite® S-102 Static Control Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Stat-Rite® S-102 is a static dissipative Polyethylene alloy. Stat-Rite® S-102 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protection. It is specially developed for blown film applications and is highly suitable for ESD-sensitive parts requiring a robust packaging that does not tear easily. Features:Clean, permanent, and more consistent than anti-statProvides protection for many yearsRobustApplications:Semiconductor packagingElectronic component packagingHard disk drive packagingAvailable in Americas, Europe, Middle East, Africa, India and AsiaPreliminary Data SheetData provided by Lubrizol.
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ASTM D792
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 15.2 MPa
2200 psi
ASTM D638
Elongation at Break >= 500 %
>= 500 %
ASTM D638
Optical Properties Metric English Comments
Haze 37 %
37 %
ASTM D1003
Transmission, Visible 84 %
84 %
ASTM D1003
Electrical Properties Metric English Comments
Volume Resistivity 8.00e+9 ohm-cm
8.00e+9 ohm-cm
ESD S11.11
Surface Resistance 4.00e+8 ohm
4.00e+8 ohm
ESD S11.11
Static Decay >= 2.0 sec
>= 2.0 sec
Charged Plate Monitor; (1000 V to 10 V)
Tribocharge 10 V
10 V
Nitrile Glove
Descriptive Properties Value Comments
Color Natural, Translucent