Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucent Polymers CPP-320 Polypropylene, 20% Calcium Carbonate Filled, Impact Modified

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Calcium Carbonate (CaCO3) Filler
Manufacturer Lucent Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucent Polymers CPP-320 Polypropylene, 20% Calcium Carbonate Filled, Impact Modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.012 cm/cm

@Thickness 3.17 mm
0.012 in/in

@Thickness 0.125 in
1/8" Section
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.69 MPa
3001 psi
ASTM D638
Elongation at Break >= 10 %
>= 10 %
ASTM D638
Flexural Strength 37.97 MPa
5507 psi
ASTM D790
Flexural Modulus 1.241 GPa
180.0 ksi
ASTM D790
Izod Impact, Notched 1.50 J/cm

@Thickness 3.17 mm
2.80 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 57.22 °C
135.0 °F
ASTM D648