Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.50 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.81 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne LubriOne™ PC-20GF/15T Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Izod Impact, Notched | 1.50 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.81 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ GF 604 35 HS Natural Polyamide 6 (Nylon 6) The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en.. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL4019 PC (Asia Pacific) Lexan* EXL4019 is an opaque 9% Glass Fiber (GF) reinforced polycarbonate (PC) siloxane copolymer resin for injection molding (IM) applications requiring improved stiffness. This resin also offers im.. |
|||
Izod Impact, Notched | 1.50 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.81 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® NN-50GF/000 Polyamide 66 (Nylon 66) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® LUX9616G PC (Asia Pacific) Lexan LUX9616G is a flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effective and thin wall FR performance. It intended to meet WEEE/RoHS requirem.. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3.. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer (Asia Pacific) Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3.. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® ML6413 PC (Asia Pacific) Lexan* ML6413 resin is an impact modified, flame retardant polycarbonate grade with Br- & Cl-free FR systems. It features improved light shielding capability with good flow, impact and thermal prope.. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer (Asia Pacific) Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
Izod Impact, Notched | 1.50 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.81 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ GF 1200 A 43 HS Natural Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | ISO 180 |
Wellman Wellamid® GFT15N050-N2 15% Impact Modified Glass Reinforced Nylon 66/6, Lubricated & Heat Stabilized
&n Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ.. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature 23.0 °C |
2.81 ft-lb/in @Temperature 73.4 °F |
V-Notched 1/8"; ASTM D256 |
Kotec Carbotex K-30F5 Polycarbonate, Wear Resistant Features: Wear resistance, TranslucentApplications: OA equipment, Communications, Precision parts, Machineries, E & E partsInformation provided by Kotec Corporation |
|||
Izod Impact, Notched | 1.50 J/cm @Thickness 3.17 mm |
2.80 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Lucent Polymers CPP-320 Polypropylene, 20% Calcium Carbonate Filled, Impact Modified Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -20.0 °C |
2.81 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR2210 PC (Europe-Africa-Middle East) LNP* Lubricomp* Lexan_WR2210 compound is based on an aternative polymeric wear technology and does not contain silicones. LEXAN WR2210 has superior processability (flow similar to LEXAN 121) and par.. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 357X PBT (Europe-Africa-Middle East) VALOX 357X is an impact modified, flame retarted PBT+PC blend. Applications like bobbins, switches and enclosures. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® V2105U PBT Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature 0.000 °C |
2.81 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® X4830 PBT+PC Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL HH180 PPE+PS (Europe-Africa-Middle East) Noryl* HH180 is a high heat, unfilled modified polyphenylene ether resin with a Vicat B/120 temperature of 185 deg C. Noryl HH180 is only available in color 80365. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® V2105U PBT (Europe-Africa-Middle East) Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |
|||
Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | ASTM D256 |
PlastxWorld Veroplas PB3300 Nylon 66 30% glass filled injection molding gradeInformation provided by PlastxWorld Inc. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature 23.0 °C |
2.81 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamShine PAS100 ASA, General Purpose General purpose injection molding ASAInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature 23.0 °C |
2.81 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamTough PZ300G6 Polycarbonate, 30% Glass Fiber 30% Glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1606 Glass Filled Chemically Coupled Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1606 is a 30% glass filled chemically coupled impact copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature 23.0 °C |
2.81 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamTough PZ300G8 Polycarbonate, 40% Glass Fiber 40% Glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | ASTM D256 |
E-Polymers TEKANATE™ G730 , 30% Glass Fiber Reinforced Poly Carbonate 30% Glass Fiber reinforcedInformation provided by E-Polymers Co. Ltd. |
|||
Izod Impact, Notched | 1.50 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
2.81 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
Notched V 10 mm; ASTM D256 |
Solvay Specialty Polymers Solef® 1012 PVDF Homopolymer
(discontinued **) Key features of this grade: High Viscosity, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-c.. |
|||
Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | ASTM 3.2mm |
Asahi Kasei Xyron® AT610 Modified Polyphenylene Ether Applications: Information provided by Asahi Kasei |
|||
Izod Impact, Notched | 1.50 J/cm @Temperature -30.0 °C |
2.81 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL5689 PC Copolymer Lexan* EXL5689 polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features UL94 V0 @ 1.5mm flame retardancy based .. |
|||
Izod Impact, Notched | 1.50 J/cm | 2.81 ft-lb/in | ASTM D256A |
LyondellBasell Astryn 6652 Polypropylene Homopolymer Key Features: low melt flow, medium modulus polypropylene homopolymer, high strength, high impact, good hydrolytic abilityApplications: water pipe fittings and connectorsDescription: Astryn 6652 low.. |