Lucite International Colacryl ® TS1785 Acrylic Dental Resin

Category Polymer , Thermoplastic , Acrylic (PMMA)
Manufacturer Lucite International
Trade Name Colacryl ®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucite International Colacryl ® TS1785 Acrylic Dental Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Cold-curing denture repair resin with Methyl Methacrylate based copolymers. Features fast polymerisation, easy mixing, good clarity, short hydroflask cure cycles, and excellent pigment acceptance.Information provided by Lucite International
Physical Properties Metric English Comments
Particle Size 45 - 55 µm
45 - 55 µm
Molecular Weight 900000 - 1.50e+6 g/mol
900000 - 1.50e+6 g/mol
Processing Properties Metric English Comments
Cure Time 20.0 min

@Pressure 0.207 MPa,
Temperature 40.0 °C
0.333 hour

@Pressure 30.0 psi,
Temperature 104 °F
Descriptive Properties Value Comments
Pour Time (min) >3
Residual peroxide (%) 0.2 - 0.5
Set Time (min) 14 - 20