Lushan H-4 Adhesive Resin for Aluminum Plastic Composite Pipe

Category Polymer , Adhesive , Thermoplastic , Polypropylene (PP)
Manufacturer Lushan
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Lushan H-4 Adhesive Resin for Aluminum Plastic Composite Pipe.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Adhesive resin Lushan series for aluminum-plastic composite pipe is maleic grafted polyethylene used for PE-AL-PE, PEX-AL-PEX and PERT-AL-PERT composite pipes. Lushan adhesive resin could provides innovative solutions for plumbing and heating pipe systems including applications of domestic water piping, under-floor heating, radiator connections and wall, cooling and heating installations, district heating and industrial piping, etc. PPR pipe adhesive resin Lushan series is maleic grafted polypropylene used for PPR piping system. Lushan makes its adhesive resin to be possible to combine the advantages of materials and polymers in the multi-layer aluminum plastic composite structures. The high mechanical and thermal cycle resistance of Lushan adhesive resin provide an excellent bonding effect over a wide temperature range. Applications: Overlapped WeldedCo-ExtrusionInformation provided by Lushan
Physical Properties Metric English Comments
Density 0.924 g/cc
0.0334 lb/in³
ASTM D1505
Melt Index of Compound 4.5 g/10 min
<br>@Load 2.16 kg
4.5 g/10 min
<br>@Load 4.76 lb
190°C/230°C; ASTM D1238
Mechanical Properties Metric English Comments
Elongation at Break 600 %
600 %
ASTM D638
Thermal Properties Metric English Comments
Melting Point 126 °C
259 °F
ASTM D2117
Vicat Softening Point 95.0 °C
203 °F
ASTM D1525