Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Hostacomâ„¢ BG749GC/1 Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Calcium Carbonate (CaCO3) Filler
Manufacturer LyondellBasell
Trade Name Hostacom™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Hostacomâ„¢ BG749GC/1 Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Hostacomâ„¢ BG749GC/1 medium melt flow, 1,100 MPa flexural modulus, UV-stabilized, precolored, 20% calcium carbonate-filled polypropylene copolymer resin has an excellent combination of stiffness and processability. It was designed primarily for applications that undergo extended outdoor exposure. Uses: Outdoor applicationsInformation provided by Basell.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ISO 1183
Melt Flow 13 g/10 min

@Load 2.16 kg,
Temperature 230 °C
13 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.0 MPa
2760 psi
ISO 527-1, -2
Elongation at Yield 7.0 %
7.0 %
ISO 527-1, -2
Flexural Modulus 1.10 GPa
160 ksi
ISO 178