Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 19.0 MPa | 2760 psi | ISO 527 |
Polyplastic Armlen® PP-10IM-901 Polypropylene, Mineral Filled Information provided by PolyPlastic Group. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | ASTM D412 |
Precision Polymer Engineering Perlast® G80T Perfluoroelastomer A black perfluoroelastomer compound with excellent steam resistance and mechanical properties. It has extremely low outgassing properties.Applications: For use in applications which require long-ter.. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® PP 1395 PRE-ELEC PP 1395 is a dissipative thermoplastic compound based on polypropylene. The electrical dissipation is achieved by using special conductive carbon black. In addition to stable surface resist.. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | ISO 527 |
Quadrant EPP Cestilene™ HD 1000 Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Tensile Strength, Yield | 19.0 - 28.0 MPa | 2760 - 4060 psi | |
Reliance Industries Polypropylene Impact Copolymer Typical properties of Reliance - Repol Polypropylene grades. Properties depend on rubber content, presence of nucleating agent, MFIInformation provided by Reliance Industries |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | ASTM D638 |
SABIC Innovative Plastics LNP FARADEX MS003 PP LNP* FARADEX* MS003 is a compound based on Polypropylene resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Tensile Strength, Yield | 19.0 MPa @Temperature 23.0 °C |
2760 psi @Temperature 73.4 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® 6359FG NC010 TPC-ET
(Unverified Data**) Hytrel® 6359FG is a medium modulus Hytrel® grade with nominal durometer hardness of 63D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing t.. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® CP 1318
(discontinued **) PRE-ELEC CP 1318 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivit.. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | 150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2 |
Solvay Engineered Polymers SEQUEL® 1440LS TPO
(discontinued **) Description: SEQUEL® 1440LS engineered polyolefin material is designed for large automotive exterior applications that require ductile impact properties at low temperatures, excellent processabilit.. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | 150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2 |
Solvay Engineered Polymers SEQUEL® 1485 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 1485 engineered polyolefin material is designed for large automotive exterior applications that require ductile impact properties at low temperatures, improved scratch and mar .. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | ASTM Data |
Americas Styrenics Styron® 489M High Impact Polystyrene
(discontinued **) STYRON® 489M high impact polystyrene resin is a high flow resin with excellent impact. When used unmodified for the manufacture of food contact articles STYRON 489M complies with the US Food, Drug .. |
|||
Tensile Strength, Yield | 19.0 - 63.0 MPa @Temperature -40.0 - 80.0 °C |
2760 - 9140 psi @Temperature -40.0 - 176 °F |
Average value: 41.0 MPa Grade Count:2 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is .. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | ASTM D638 |
LyondellBasell Montell 1900CM UHMW Polyethylene Key Features: ultrahigh molecular weight polyethylene resin, excellent abrasion resistance, high impact strength, low coefficient of fraction, good chemical resistance, low odor and taste transfer, .. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | 50 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 2-3302 TO BU Elastomer Modified, UV-Stabilized Polypropylene Block-Copolymer INNOPOL® CS 2-3302 TO BU is an elastomer modified, UV-stabilized compound based on polypropylene block-copolymer.INNOPOL® CS 2-3302 TO BU is developed for producing injection molded automotive.. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | 50 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 2-8960 60% Barium-Sulfate Filled Polypropylene Block-Copolymer INNOPOL® CS 2-8960 is a 60% Barium-sulfate filled compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-8960 is developed for.. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON TX06488NTX1 PU LNP* STAT-KON* TX06488NTX1 is a compound based on Polyurethane resin containing Proprietary Filler(s). Added features of this grade are: Execllent Ductility, Electrically Conductive. |
|||
Tensile Strength, Yield | 19.0 MPa @Temperature 80.0 °C |
2760 psi @Temperature 176 °F |
ISO Data |
Styrolution Luran® S 757 G ASA Luran S 757 G is an easy flowing injection molding ASA grade with large flow path/wall thickness ratios.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP MH0500C PP (Asia Pacific) LNP* Thermocomp* MH0500C is a compound based on Polypropylene resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | ISO 527 |
SABIC Innovative Plastics LNP Thermocomp MB008S PP (Asia Pacific) LNP* Thermocomp* MB008S is a compound based on Polypropylene resin containing Glass Bead. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Pa.. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP MH0500C PP LNP* THERMOCOMP* MH0500C is a compound based on Polypropylene resin. Added feature of this material is: High Specific Gravity. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | ISO 527 |
Unipetrol PE HD LITEN® VL 20 HDPE Extrusion and pipe applications.Information provided by Unipetrol RPA |
|||
Tensile Strength, Yield | >= 19.0 MPa | >= 2760 psi | Requirement |
Westlake Plastics Lennite® GUR1050 (Type II) Ultra-high Molecular Weight Polyethylene For Medical Applications Medical grade Lennite UHMWPE is produced from premium resins in accordance with ASTM specification F648 and International Standard ISO 5834-1 for surgical implants. Westlake Plastics' proprietary m.. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | ISO 527-2 |
ExxonMobil Exxtral™ BMV 201 Performance Polyolefin Product Description: A specialty thermoplastic olefin injection molding compound resin with good flow, cold temperature impact resistance, low CLTE, and excellent paintability for large automotive e.. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | |
Dow DOWLEX™ IP-50 High Density Polyethylene DOWLEX® IP-50 resin is an improved processing high density polyethylene resin with controlled molecular weight distribution designed for thin wall food containers. This resin is recommended for flo.. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | 50 mm/min; ASTM D638 |
Carmel Olefins CAPILENE® TR 50 Polypropylene Impact Copolymer Description: CAPILENE® TR 50 is a medium melt flow rate heterophasic copolymer with very high impact strength, even at low temperature, designed for injection molding. This grade combines good pr.. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | |
BASF Novolen® 2600 TC Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | ASTM D638 |
Huntsman Rexell® H2103 Injection Molding LLDPE
(discontinued **) Linear-low medium density homopolymer, injection molding, FDA compliant.Features: Good ESCR, low taste and order.Applications: Containers, closures, and ideal for blends and non-carbonated beverage .. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | 2 in/min; ASTM D638 |
Solvay Engineered Polymers DEXFLEX® 880-1 TPO
(discontinued **) Description: DEXFLEX® 880-1 is a thermoplastic olefinic elastomer (TPO) designed for exterior automotive applications requiring a combination of stiffness, low-temperature impact, good processabili.. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | ASTM D638 |
LyondellBasell Hifax™ ETA-3163UV Thermoplastic Olefin Resin Key Features: medium melt flow, medium high modulus, UV-stabilized thermoplastic olefin resin, excellent impact and stiffness balance, excellent weatherability, good processabilityApplications: mold.. |
|||
Tensile Strength, Yield | 19.0 MPa | 2760 psi | 2.0 in/min; ASTM D638 |
Ineos Nova Zyntar® 779 High Performance Flame Retardant Polystyrene
(discontinued **) Non-Decabromodiphenyl Oxide, Color stable, Custom colorsApplications: Injection molding, Alternative to flame retardant ABS, Copiers, Computer monitors, Office equipmentThis is an impact grade of po.. |