Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer LyondellBasell
Trade Name Pro-fax
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Pro-fax PD702 Polypropylene Homopolymer, High Flow.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Primary Processing Method: Injection MoldingKey Features: high flow polypropylene homopolymer resin for injection molding, FDA acceptable, ease of processing allows increased design freedom and higher productivity, excellent dimensional stability, processes with low built-in stress, good surface finish colorApplications: chemical containers and lids, large flat trays, thin complex parts, shipping containersMeets FDA requirements in 21 CFR 177.1520 for all food contact applications up to 212°F (100°C).Description: Pro-fax PD702 high flow, controlled rheology polypropylene homopolymer resin is designed for injection molding. It is available in pellet form. It meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirements of TSCA and DSL.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792B
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 89
89
ASTM D785A
Tensile Strength, Yield 32.0 MPa
4640 psi
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus 1.20 GPa
174 ksi
1% secant at 0.05 in/min; ASTM D790A
Izod Impact, Notched 0.320 J/cm
0.599 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
ASTM D648
Users viewing this material also viewed the following: