Material Notes:
Key Features: nucleation shortens cycles for higher productivity, resists dirt and dust pick-up, good cold impact resistance, good stiffness and impact balance, high flow for ease of mold filling and minimum warpage, low odor and taste transfer, FDA acceptableApplications: dairy containers, housewares and consumer productsMeets FDA requirements in 21 CFR 177.1520 for all food contact, excluding cooking applications.Description: Pro-fax SV954 easy molding, fully formulated, high melt flow, medium impact polypropylene copolymer resin is designed for thin-wall applications requiring an excellent balance of stiffness and impact resistance. It is available in pellet form. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.1520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirements of TSCA and DSL.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792B
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.0 MPa
3920 psi
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Flexural Modulus 1.40 GPa
203 ksi
1% secant at 0.05 in/min; ASTM D790A
Izod Impact, Notched 0.730 J/cm
1.37 ft-lb/in
ASTM D256A
Impact Test 21.0 J

@Temperature 5.00 °C
15.5 ft-lb

@Temperature 41.0 °F
Montell drop weight impact strength
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 115 °C
239 °F
ASTM D648