LyondellBasell SEQUEL® 1780 Engineered Polyolefin

Category Polymer , Thermoplastic , Polyolefin
Manufacturer LyondellBasell
Trade Name SEQUEL®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell SEQUEL® 1780 Engineered Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: SEQUEL® 1780 engineered polyolefin is designed for mold-in-color or partially painted automotive exterior applications that require dimensional stability over a broad temperature range with enhanced scratch and mar resistance. This material exhibits excellent processability and low-temperature properties. Applications: Bumper side claddings, rockers, and other components that demand close dimensional tolerances Information provided by Solvay Engineered Polymers.LyondellBasell acquired Solvay Engineered Polymers in 2008.
Physical Properties Metric English Comments
Specific Gravity 1.01 g/cc
1.01 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
as molded; ISO 294
Melt Flow 21 g/10 min
21 g/10 min
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.0 MPa
2900 psi
50 mm/min; ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
I.B., TAN, 0.5 in/min; ASTM D790
Thermal Properties Metric English Comments
CTE, linear 52.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
28.9 µin/in-°F

@Temperature -22.0 - 176 °F
ASTM E228