Material Notes:
Fine-grained reaction-bonded SiC. Used for mechanical seals and other SiC applications that require a high surface finish/tight tolerances. Si content can be tailored for the application.Information provided by M Cubed Technologies, Inc.
Physical Properties Metric English Comments
Density 3.00 g/cc
0.108 lb/in³
ASTM C135
Mechanical Properties Metric English Comments
Knoop Microhardness 1080

@Load 2.00 kg
1080

@Load 4.41 lb
kg/mm2; ASTM C1326
Modulus of Elasticity 330 GPa
47900 ksi
ASTM E494
Flexural Strength 350 MPa
50800 psi
ASTM C1161
Poissons Ratio 0.18
0.18
ASTM E494
Fracture Toughness 4.00 MPa-m½
3.64 ksi-in½
ASTM C1421
Shear Modulus 140 GPa
20300 ksi
Calculated
Thermal Properties Metric English Comments
CTE, linear 3.00 µm/m-°C

@Temperature 25.0 - 100 °C
1.67 µin/in-°F

@Temperature 77.0 - 212 °F
ASTM E831
Thermal Conductivity 150 W/m-K
1040 BTU-in/hr-ft²-°F
ASTM E1461
Descriptive Properties Value Comments
Matrix SiC
Particle Reinforcement SiC
Vol. % Reinforcement 70