Material Notes:
Features: High Flow, High Impact Resistance, Good StiffnessUses: Automotive Interior Parts, Closures, Household Goods, ToysApprovals: FDA 21 CFR 177.1520 Processing Method: Injection MoldingInformation provided by M. Holland.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 88
88
ASTM D785
Tensile Strength, Yield 24.1 MPa
3500 psi
Type I, 2 in/min; ASTM D638
Elongation at Break 55 %
55 %
Type I, 2 in/min; ASTM D638
Flexural Modulus 1.17 GPa
170 ksi
at 0.05 in/min; ASTM D790
Izod Impact, Notched 0.961 J/cm
1.80 ft-lb/in
at 73°F; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 93.3 °C
200 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 51.7 °C
125 °F
Unannealed; ASTM D648
Descriptive Properties Value Comments
Form Pellets