Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

M. Holland Company IS410 Polystyrene, High Impact  (discontinued **)

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M. Holland Company IS410 Polystyrene, High Impact  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Good Colorability, High Flow, Impact ModifiedUses: Household Goods, Modeling Material, ToysApprovals: FDA 21 CFR 177.1520Processing Method: Injection MoldingInformation provided by M. Holland.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Melt Flow 13 g/10 min

@Load 5.00 kg,
Temperature 200 °C
13 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.5 MPa
3550 psi
ASTM D638
Elongation at Break 40 %
40 %
ASTM D638
Flexural Strength 46.9 MPa
6800 psi
at 10 in/min; ASTM D790
Flexural Modulus 2.55 GPa
370 ksi
at 10 in/min; ASTM D790
Izod Impact, Notched 0.694 J/cm
1.30 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 87.8 °C
190 °F
Unannealed; ASTM D648
Descriptive Properties Value Comments
Form Pellets