Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 24.5 MPa | 3550 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ PPH-40C Nat Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Tensile Strength, Yield | 24.5 MPa | 3550 psi | ASTM D638 |
Resirene Resirene® 2220 Medium Impact Polystyrene Features:High FlowEasy ProcessingGood GlossHigh Tensile ModulusFDA Rating: 21 CFR 177.1640High ProductivityExternal LubricatedApplications:InjectionThin Wall ApplicationsHard to Fill MoldsHangersVid.. |
|||
Tensile Strength, Yield | 24.5 MPa | 3550 psi | ASTM D638 |
M. Holland Company IS410 Polystyrene, High Impact
(discontinued **) Features: Good Colorability, High Flow, Impact ModifiedUses: Household Goods, Modeling Material, ToysApprovals: FDA 21 CFR 177.1520Processing Method: Injection MoldingInformation provided by M. Holl.. |
|||
Tensile Strength, Yield | 24.5 MPa | 3550 psi | aged in air at 100ºC for 4 days |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with Hercoflex 600 Plasticizer MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 24.5 MPa | 3550 psi | ASTM D638 |
Lotte Chemical Titan TITANPRO® EPC40R Polypropylene impact copolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Tensile Strength, Yield | 24.5 MPa | 3550 psi | ASTM D638 |
Lotte Chemical Titan TITANPRO® SM340 Polypropylene impact copolymer Titanpro® SM340 is an intermediate impact material. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The adju.. |
|||
Tensile Strength, Yield | 24.5 MPa | 3550 psi | ASTM D638 |
Lotte Chemical Titan TITANPRO® SM850 Polypropylene impact copolymer Titanpro® SM850 is a nucleated extra high flow material. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The.. |
|||
Tensile Strength, Yield | 24.5 MPa | 3550 psi | ASTM D638 |
Lotte Chemical Titan TITANPRO® SM950 Polypropylene impact copolymer Titanpro® SM950 is a nucleated extra high flow material. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The.. |
|||
Tensile Strength, Yield | 24.5 MPa | 3550 psi | ASTM D1238 |
Iran Petrochemical (PCC) 7000F High Density Polyethylene 7000F is a high density polyethylene for enhanced ultra thin film.Information provided by Iran Petrochemical Commercial Co. |
|||
Tensile Strength, Yield | 24.5 MPa | 3550 psi | ASTM D638 |
Tipco Tipcolene® CR 7228 - 30% Talc/Mineral Reinforced Polypropylene Copolymer 30% Mineral Reinforced PP CopolymerApplications: Automotive DashboardsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Tensile Strength, Yield | 24.5 MPa | 3550 psi | ASTM D638 |
Tipco Tipcolene® FPC 20 PPC - 20% Calcium Carbonate Reinforced Polypropylene Copolymer 20% Calcium Carbonate Filled PP CopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India. |
|||
Tensile Strength, Yield | 24.5 MPa | 3550 psi | ASTM D638 |
Tipco Tipcolene® FPC 40 - 40% Calcium Carbonate Reinforced Polypropylene Homopolymer 40% Calcium Carbonate Filled PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Tensile Strength, Yield | 24.5 MPa | 3550 psi | ASTM D638 |
Tipco Tipcolene® FPDZ-1000 - 25% Talc/Mineral Reinforced Polypropylene Copolymer, High Stiffness & Impact Strength Mineral Reinforced, High Stiffness, High Impact PP CopolymerApplications: Automotive DashboardsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Tensile Strength, Yield | 24.5 MPa | 3550 psi | aged in air at 100ºC for 4 days |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with Hercoflex 600 Plasticizer MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tensile Strength, Yield | 24.5 MPa | 3550 psi | ASTM Data |
Dow AIM® 4810 High Impact Styrenic Resin AIM® 4810 advanced styrenic resin is designed to offer the processability of high impact polystyrene and the gloss and practical toughness of high gloss ABS. It can be processed at lower temperatur.. |
|||
Tensile Strength, Yield | 24.5 MPa | 3550 psi | ASTM D-638 |
Bapolan® 6403 Polystyrene, Extrusion Grade Bapolan PS6403 is a high impact polystyrene resin designed for extrusion-thermoforming applications. It complies with US FDA21 CFR177.1640 and 94HB UL rating.Applications: General purpose, housewar.. |
|||
Tensile Strength, Yield | 24.5 MPa @Strain <=1.00 % |
3550 psi @Strain <=1.00 % |
Silicone Property; Arlon-SAQ-TMS-008 |
Arlon CP-594CX Bulk Compound Product Use: Electrically insulating electronic adhesive. Bonds without primer.Appearance: Gray, high viscosity gumUL94V-0: The product is designed to meet UL94V-0 flame resistance requirements but .. |
|||
Tensile Strength, Yield | 24.5 MPa @Strain <=1.00 % |
3550 psi @Strain <=1.00 % |
Silicone Property; Arlon SQA-TMS-008 |
Arlon Thermabond® 48A43X008 0.008"(0.203 mm) Cured Silicone Rubber with Fiberglass Substrate Description: Thermabond® Electrically insulating, thermally conductive, thermal interface material (TIM).Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1080 FiberglassSide 2: Cu.. |
|||
Tensile Strength, Yield | 24.5 MPa @Strain <=1.00 % |
3550 psi @Strain <=1.00 % |
Silicone Property; Arlon SQA-TMS-008 |
Arlon Thermabond® 48A51X015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Primerless Thermabond® Electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner 1: Polyethylene Side 1: Uncured Silicone Rubb.. |
|||
Tensile Strength, Yield | 24.5 MPa @Strain <=1.00 % |
3550 psi @Strain <=1.00 % |
Arlon SQA-TMS-008 |
Arlon Thermabond® 51A42X012 0.012" (0.305 mm) Cured Silicone Rubber with Fiberglass Substrate Description: Thermabond® - Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction: Liner: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 7628.. |
|||
Tensile Strength, Yield | 24.5 MPa @Strain <=1.00 % |
3550 psi @Strain <=1.00 % |
Silicone Property; Arlon SQA-TMS-008 |
Arlon Thermabond® R37623X008 0.0050" Cured Silicone Rubber with Fiberglass Substrate Thermabond®: Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction:Side 1: Cured Silicone RubberSubstrate: 1080-style FiberglassSide 2: Cured Silico.. |
|||
Tensile Strength, Yield | 24.5 MPa | 3550 psi | 50 mm/min |
Arkema Group Appryl® 3120 MU 5 Polypropylene - Polyethylene Copolymer PP/PE copolymer Colored directly or during the injection molding process. This grade with a very good impact test, has been developed for interior trim automotive applications. It is UV stabilized.I.. |
|||
Tensile Strength, Yield | 24.5 MPa | 3550 psi | ASTM D638 |
Tipco Tipcolene® ISL 10 BX1 - 10% Talc/Mineral Reinforced Polypropylene Homopolymer, High Flow, Stiffness & Impact Strength 10% Mineral Reinforced, High Stiffness, High Impact PP HomopolymerApplications: Automotive InteriorsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
Indi.. |
|||
Tensile Strength, Yield | 24.5 MPa | 3550 psi | ASTM D638 |
Tipco Tipcolene® FPDG-M FPDG M - 28% Talc/Mineral Reinforced Polypropylene Copolymer, High Stiffness & Impact Strength Mineral Reinforced, High Stiffness, High Impact PP CompoundApplications: Automotive DashboardsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Tensile Strength, Yield | 24.5 MPa | 3550 psi | 50 mm/min; ASTM D638 |
Amco PRIMATOP PP CO 220-23 Impact Polypropylene Copolymer PP CO 220-23 has easy mold flow and excellent dimensional stability. Applications include closures, housewares, and small appliance applications.Former A-Top Polymers product; part of Amco product l.. |
|||
Tensile Strength, Yield | 24.5 MPa @Strain <=1.00 % |
3550 psi @Strain <=1.00 % |
Silicone Property; ASTM E 831 |
Arlon R37480X008 0.008" (0.203 mm) Uncured Silicone Rubber with Substrate: PTFE Coated Fiberglass Substrate Description: Primerless Thermabond® electrically insulating, thermally conductive, electronic adhesive. Bonds without primer.Design/Construction: Liner: FEP Add-on: Uncured Silicone Rubber Substra.. |
|||
Tensile Strength, Yield | 24.5 MPa @Strain <=1.00 % |
3550 psi @Strain <=1.00 % |
Silicone Property; ASTM E 831 |
Arlon R37622X008 0.008" (0.203 mm) Cured Silicone Rubber with Release PET Carrier Description: Thermabond® electrically insulating, thermally conductive, thermal interface materialDesign/Construction: Liner: Polyethylene Product: Cured Silicone Rubber Carrier: PTFE Coated Fiber.. |
|||
Tensile Strength, Yield | 24.5 MPa @Strain <=1.00 % |
3550 psi @Strain <=1.00 % |
Silicone Property; ASTM E 831 |
Arlon R37622X014 0.014" (0.356 mm) Cured Silicone Rubber Description: Thermabond® electrically insulating, thermally conductive, thermal interface material. Design/Construction: Liner: Polyethylene Product: Cured Silicone Rubber Carrier: PTFE Coated Fib.. |