Material Notes:
Good impact resistanceGood mold releaseHigh viscosityApplications: AppliancesProtective coveringsDecorative displaysHousings
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
23/23°C; ASTM D792
Melt Flow 6.0 g/10 min
6.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 72.4 MPa
10500 psi
ASTM D638
Tensile Strength, Yield 60.0 MPa
8700 psi
ASTM D638
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
(0.125 in); ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 142 °C
288 °F
Annealed; ASTM D648
Descriptive Properties Value Comments
Characteristics Mold release
Forms Pellets
Processing Methods Injection molding