Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

MMCC Al/Al2O3 Short Fiber Aluminum Matrix Composite

Category Ceramic , Oxide , Aluminum Oxide , Metal , Metal Matrix Composite , Nonferrous Metal , Aluminum Alloy
Manufacturer Metal Matrix Cast Composites (MMCC)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MMCC Al/Al2O3 Short Fiber Aluminum Matrix Composite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC).
Physical Properties Metric English Comments
Density 3.10 g/cc
0.112 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 300 - 450 MPa
43500 - 65300 psi
Modulus of Elasticity 120 - 140 GPa
17400 - 20300 ksi
Youngs Modulus
Fracture Toughness 15.0 - 20.0 MPa-m½
13.7 - 18.2 ksi-in½
Thermal Properties Metric English Comments
CTE, linear 17.0 µm/m-°C

@Temperature 20.0 °C
9.44 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 100 W/m-K
694 BTU-in/hr-ft²-°F
Copyright © lookpolymers.com All Rights Reserved