MMCC Aluminum/Al2O3 55p Aluminum Matrix Composite

Category Metal , Metal Matrix Composite , Nonferrous Metal
Manufacturer Metal Matrix Cast Composites (MMCC)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MMCC Aluminum/Al2O3 55p Aluminum Matrix Composite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC).
Physical Properties Metric English Comments
Density 3.46 g/cc
0.125 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Yield 380 MPa
55100 psi
Modulus of Elasticity 167 GPa
24200 ksi
Thermal Properties Metric English Comments
CTE, linear 13.2 µm/m-°C

@Temperature 20.0 °C
7.33 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.831 J/g-°C
0.199 BTU/lb-°F
Thermal Conductivity 88.5 W/m-K
614 BTU-in/hr-ft²-°F