Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Magyar Aluminum ALOLT 120F Aluminum Hydroxide

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Magyar Aluminium
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Magyar Aluminum ALOLT 120F Aluminum Hydroxide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fine Precipitated Type
Physical Properties Metric English Comments
Bulk Density 0.250 - 0.400 g/cc
0.00903 - 0.0145 lb/in³
Brightness >= 98.5 %
>= 98.5 %
Whiteness
Particle Size 0.80 - 1.5 µm
0.80 - 1.5 µm
d50
Specific Surface Area 8.0 - 12 m²/g
8.0 - 12 m²/g
BET
Component Elements Properties Metric English Comments
Fe2O3 <= 0.020 %
<= 0.020 %
SiO2 <= 0.020 %
<= 0.020 %
Electrical Properties Metric English Comments
Electrical Resistivity <= 5000 ohm-cm
<= 5000 ohm-cm
Processing Properties Metric English Comments
Moisture Content <= 0.50 %
<= 0.50 %
Descriptive Properties Value Comments
Aluminum Hydroxide (%) >99.4
Determined by difference
Users viewing this material also viewed the following: