Material Notes:
Applications: Rovene® 6126 provides a flexible yet strong cohesive bond for a range of materials and particle surface areas. Rovene® 6126 imparts films with good water resistance properties. For use in the following application areas: Quarries Mines (particularly coal) Stockpiles Landfills Unpaved Roads Material/Mineral TransportStorage and Handling: Protect from freezing. Ideal storage temperature is 22°C (72°F). Read the Rovene® 6126 Material Safety Data Sheet before handling, storing, or using this product.Information provided by Mallard Creek Polymers
Physical Properties Metric English Comments
Solids Content 39.5 - 40.5 %
39.5 - 40.5 %
Particle Size 0.18 µm
0.18 µm
pH 4.0 - 5.0
4.0 - 5.0
Brookfield Viscosity <= 500 cP
<= 500 cP
#20/200
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 20.0 °C
68.0 °F
Descriptive Properties Value Comments
Emulsifiers Anionic