Physical Properties Metric English Comments
Particle Size 0.18 µm
0.18 µm
Mallard Creek Polymers ROVENE® 4019 SBR Latex
ROVENE® 4019 is a carboxylated styrene-butadiene emulsion that has a firm hand with excellent strength properties. This binder is a low VOC containing latex that is cross-linkable with external c..
Particle Size 0.18 µm
0.18 µm
Mallard Creek Polymers ROVENE® 4180 SBR Latex
ROVENE® 4180 is a carboxylated styrene-butadiene emulsion that has a firm hand with excellent strength properties. This binder is a low VOC containing latex that is cross-linkable with external ..
Particle Size 0.18 µm
0.18 µm
Mallard Creek Polymers ROVENE® 4487 SBR Latex
ROVENE® 4487 is a carboxylated styrene-butadiene emulsion that has a firm hand with excellent strength properties. This binder is a low VOC containing latex that is cross-linkable with external ..
Particle Size 0.18 µm
0.18 µm
Mallard Creek Polymers ROVENE® 6014 Acrylic Emulsion
Applications: Rovene® 6014 is a self crosslinking acrylic polymer providing a stiff hand to frothed or saturated substrates. Rovene® 6014 is recommended for various nonwoven and paper applicat..
Particle Size 0.18 µm
0.18 µm
Mallard Creek Polymers Rovene® 6126 Styrene-Acrylic Emulsion
Applications: Rovene® 6126 provides a flexible yet strong cohesive bond for a range of materials and particle surface areas. Rovene® 6126 imparts films with good water resistance properties. F..
Particle Size 0.18 µm
0.18 µm
Mallard Creek Polymers Tykote® 1019 Styrene-Butadiene Emulsion
Tykote® 1019 is a carboxylated styrene-butadiene emulsion that has a firm hand with excellent film strength properties. It is intended for use as a base polymer in the formulation of barrier coat..
Particle Size 0.18 µm
0.18 µm
Average
Daikin POLYFLON LDW-40 PTFE Low Polymer, Milky Liquid
Milky liquid.Major Uses: Additive to give water repellency to water base paints.Information provided by Daikin Industries.
Particle Size 0.18 µm
0.18 µm
Mallard Creek Polymers ROVENE® 4457 SBR Latex
ROVENE® 4457 is a highly carboxylated styrene-butadiene emulsion that has a firm hand with excellent strength properties. This binder is a low VOC containing latex that is crosslinkable with extern..