Material Notes:
Rovene® 6202 is a solution version of Rovene® 6201 solid styrene-acrylic resin neutralized with ammonia hydroxide. It can be used as a pigment dispersant resin and as a modifying additive in inks or overprint varnishes. Rovene® 6202 is a general use resin solution that is used as a grinding resin to produce pigment dispersions. The solution can also be used as an additive to modify certain properties of an ink or overprint varnish. The addition of Rovene® 6202 will increase gloss, increase block resistance and improve resolubility on press. The solution can also be crosslinked due to the carboxyl functionality of the styrene-acrylic resin. Storage and Handling: Protect from freezing. Ideal storage temperature is 22°C (72°F). Read the Rovene® 6202 Material Safety Data Sheet before handling, storing, or using this product.Information provided by Mallard Creek Polymers
Physical Properties Metric English Comments
Volatiles 68 - 70 %
68 - 70 %
pH 8.1 - 8.8
8.1 - 8.8
Molecular Weight 7000 g/mol
7000 g/mol
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 120 °C
248 °F
Chemical Properties Metric English Comments
Total Acid Number 218
218
[mgKOH/g]