Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Mapal Plastics Maplon Type K OPAQLON COO1 Polypropylene Sheet

Category Polymer , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Sheet/Thermoforming Grade
Manufacturer Mapal Plastics
Trade Name Maplon
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mapal Plastics Maplon Type K OPAQLON COO1 Polypropylene Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Maplon Catalog No. L050-C001K0101 is an extremely opaque white sheet. Sheet surface is smoothly embossed with similar finish on both sides..Main advantages: High opacity, High rigidity high thermal and chemical resistance, Good weather resistance, No yellowing after exposure to light, Good print-ability in all printing methods: offset UV and conventional, screen UV and solvent basedMain disadvantages: Due to sheet hardness it requires high pressure in die cutting, Material is not recommended for box production
Physical Properties Metric English Comments
Specific Gravity 0.960 g/cc
0.960 g/cc
Thickness 500 microns
19.7 mil
Surface Tension >= 48 dynes/cm
>= 48 dynes/cm
Corona treated on both sides, After 2 months from production in original packaging
Mechanical Properties Metric English Comments
Hardness, Shore D 72
72
ISO/R 868
Film Tensile Strength at Yield, MD 37.0 MPa

@Temperature 23.0 °C
5370 psi

@Temperature 73.4 °F
ASTM D638
Film Tensile Strength at Yield, TD 36.0 MPa

@Temperature 23.0 °C
5220 psi

@Temperature 73.4 °F
ASTM D638
Film Elongation at Break, MD 50 %

@Temperature 23.0 °C
50 %

@Temperature 73.4 °F
ASTM D638
Film Elongation at Break, TD 16 %

@Temperature 23.0 °C
16 %

@Temperature 73.4 °F
ASTM D638
Film Elongation at Yield, MD 15 %

@Temperature 23.0 °C
15 %

@Temperature 73.4 °F
ASTM D638
Film Elongation at Yield, TD 12 %

@Temperature 23.0 °C
12 %

@Temperature 73.4 °F
ASTM D638
Modulus of Elasticity 0.570 GPa

@Temperature 23.0 °C
82.7 ksi

@Temperature 73.4 °F
MD/TD; ASTM D638
Tear Strength <= 230 kN/m
<= 1310 pli
Mapal internal
Thermal Properties Metric English Comments
Vicat Softening Point 155 °C
311 °F
ASTM D1525
Heat Distortion Temperature 110 °C
230 °F
ASTM 648
Optical Properties Metric English Comments
Transmission, Visible >= 99.5 %
>= 99.5 %
Measured in daylight
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved