MarkeTech 96-3-1 Tungsten Alloy, AMS-T-21014 Class 3

Category Metal , Nonferrous Metal , Refractory Metal , Tungsten Alloy
Manufacturer MarkeTech
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MarkeTech 96-3-1 Tungsten Alloy, AMS-T-21014 Class 3.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of steel and are more than 50% heavier than lead. Due to their high density, tungsten alloys offer greater radiation shielding than lead and are non-toxic. Tungsten alloys are electrically and thermal conductive and offer good corrosion resistance. They also have a low coefficient of expansion and have a high modulus of elasticity. Because of these unique properties tungsten alloys are used extensively in military applications, balance weights, aircraft components, nuclear and medical shields, fishing and sport tackle, rocket components, tool vibration dampers, electrical contacts, etc.Applications:Nuclear and medical radiation shielding for x-ray and shields for radiation therapy and industrial applications.Aircraft and helicopter rotor balance weightsInstrument balance weightsWeights for sport equipmentTool damping cutter barsHigh voltage contactsInformation provided by MarkeTech International.
Physical Properties Metric English Comments
Density 18.3 g/cc
0.661 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 28 - 34
28 - 34
Sintered Only
37 - 47
37 - 47
Swaged after Sintering
Tensile Strength, Ultimate 920 - 1100 MPa
133000 - 160000 psi
Sintered Only
1150 - 1300 MPa
167000 - 189000 psi
Swaged after Sintering
Tensile Strength, Yield 800 - 1050 MPa
116000 - 152000 psi
Swaged after Sintering
Elongation at Break 3 - 8 %
3 - 8 %
Swaged after Sintering
8 - 20 %
8 - 20 %
Sintered Only
Impact 10
10
J/cm²; Swaged after Sintering
27
27
J/cm²; Sintered Only
Component Elements Properties Metric English Comments
Iron, Fe 1 %
1 %
Nickel, Ni 3 %
3 %
Tungsten, W 96 %
96 %