Master Bond UV10FL-1 Flexibilized One Component UV Curable Adhesive

Category Polymer , Adhesive , Thermoset
Manufacturer Master Bond Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond UV10FL-1 Flexibilized One Component UV Curable Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Master Bond UV10FL-1 is a one component UV curable modified compounds, ready for use as supplied, for high performance casting and bonding applications. UV10FL-1 is a flexibilized system; it exhibits a higher tensile strength and stiffness along with excellent resistance to mechanical shock and vibration.
Physical Properties Metric English Comments
Viscosity 600 - 700 cP

@Temperature 23.0 °C
600 - 700 cP

@Temperature 73.4 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 45 - 50
45 - 50
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Descriptive Properties Value Comments
Color Light Amber; Clear