Materion Alloy M65 (C17465) Beryllium Copper Rod

Category Metal , Nonferrous Metal , Beryllium Alloy , Copper Alloy
Manufacturer Materion Corporation (former Brush Wellman)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Materion Alloy M65 (C17465) Beryllium Copper Rod.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Alloy M65 (C17465) is a machinable, high-performance, copper beryllium rod alloy from Brush Wellman. M65 has excellent strength, conductivity, and resistance to elevated temperature stress relaxation. The machinability of M65 is 80% of free machining brass. M65 is pre-hardened - No heat treatment is required after machining.Information supplied by Brush Wellman Engineered Materials.Brush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.
Physical Properties Metric English Comments
Density 8.94 g/cc
0.323 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 24
24
Hardness, Vickers 260
260
Tensile Strength, Ultimate >= 896 MPa
>= 130000 psi
Tensile Strength, Yield >= 827 MPa
>= 120000 psi
Elongation at Break 8 %
8 %
Modulus of Elasticity 138 GPa
20000 ksi
Thermal Properties Metric English Comments
Thermal Conductivity 225 W/m-K
1560 BTU-in/hr-ft²-°F
Melting Point 1030 °C
1880 °F
Component Elements Properties Metric English Comments
Beryllium, Be 0.20 - 0.50 %
0.20 - 0.50 %
Copper, Cu 97.5 - 98.6 %
97.5 - 98.6 %
As remainder
Lead, Pb 0.20 - 0.60 %
0.20 - 0.60 %
Nickel, Ni 1.0 - 1.4 %
1.0 - 1.4 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000382 ohm-cm
0.00000382 ohm-cm
Conductivity is 45% IACS
Magnetic Permeability 0.99997
0.99997
Descriptive Properties Value Comments
Machinability (% of C36000) 80%
Stress Relaxation 72%
at 200°C for 1000 hr
81%
at 175°C for 1000 hr
86%
at 150°C for 1000 hr
90%
at 125°C for 1000 hr