MetalTek MTEK ALLOY X Cast UNS N06002 Severe Corrosion and Heat Resistant Alloy

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer MetalTek
Trade Name MTEK
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MetalTek MTEK ALLOY X Cast UNS N06002 Severe Corrosion and Heat Resistant Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MetalTek
Mechanical Properties Metric English Comments
Hardness, Brinell 170
170
Tensile Strength, Ultimate >= 380 MPa
>= 55100 psi
Tensile Strength, Yield >= 240 MPa
>= 34800 psi
Elongation at Break >= 8.0 %
>= 8.0 %
Component Elements Properties Metric English Comments
Carbon, C <= 0.10 %
<= 0.10 %
Chromium, Cr 20.5 - 23 %
20.5 - 23 %
Cobalt, Co 0.50 - 2.5 %
0.50 - 2.5 %
Iron, Fe 17 - 20 %
17 - 20 %
Manganese, Mn <= 1.0 %
<= 1.0 %
Molybdenum, Mo 8.0 - 10 %
8.0 - 10 %
Nickel, Ni 41.4 - 53.8 %
41.4 - 53.8 %
As Balance
Silicon, Si <= 1.0 %
<= 1.0 %
Tungsten, W 0.20 - 1.0 %
0.20 - 1.0 %
Descriptive Properties Value Comments
Heat Treatment Sol. Anneal