Michelman® Michem® Dispersion 91530 Acrylic resin dispersion

Category Fluid , Other Engineering Material , Additive/Filler for Polymer , Polymer
Manufacturer Michelman®
Trade Name Michem® Dispersion
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Michem® Dispersion 91530 Acrylic resin dispersion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Michem® Dispersion 91530 is an additive used as a leveling aid, gloss enhancer and for buffability and mar resistance for the floor finish industry. This product is also effective for gloss enhancement for auto polish formulas.Food Contact Information when manufactured in the USA and Singapore:FDA:175.105: Components of adhesives.175.300: Resinous and polymeric components of coatings. (Restricted)175.320: Resinous and polymeric components of coatings for polyolefin films. (Restricted)176.170: Components of paper and paperboard in contact with aqueous and fatty foods. (Restricted)176.180: Components of paper and paperboard in contact with dry foods.Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 1.04 - 1.06 g/cc
1.04 - 1.06 g/cc
Volatiles 69 - 71 %
69 - 71 %
pH 8.2 - 9.7
8.2 - 9.7
Brookfield Viscosity 200 - 1000 cP
200 - 1000 cP
Spindle # 3, rpm 60
Descriptive Properties Value Comments
Appearance White to light yellow, translucent liquid
Solids Type Acrylic Resin