Michelman® Michem® Lube 190 Anionic polyethylene wax emulsion

Category Fluid , Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Michelman®
Trade Name Michem® Lube
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Michem® Lube 190 Anionic polyethylene wax emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Anionic polyethylene wax emulsionUsage: Michem® Lube 190 provides mar and scratch resistance as well as improved water resistance and is useful in the coatings and graphic arts industries.Compatible with ingredients used in many industries, including: Automotive care products; Building materials; Can and coil coatings; Concrete; Cordage and twine; Deck stains and sealants; Die lubricants; Fiber sizings; Floor polishes; Furniture coatings; Glass; Gloves, balloons, footwear and mechanical seals; Inks; Packaging films; Pressure-sensitive adhesives; Textiles; Urethane foam and VarnishesWhen manufactured in Belgium Product meets food contact regulations for: Europe: Euro. Res. AP(2004)1 (Restricted)Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.980 - 1.00 g/cc
0.980 - 1.00 g/cc
Volatiles 64.5 - 65.5 %
64.5 - 65.5 %
pH >= 7.0
>= 7.0
Recommended pH of system
8.7 - 9.7
8.7 - 9.7
Brookfield Viscosity <= 50 cP
<= 50 cP
Spindle # 2, rpm 60
Descriptive Properties Value Comments
Appearance Amber, translucent liquid
Emulsifier Charge Anionic
Solids Type High Density Polyethylene