Material Notes:
Fully Heat and UV stabilizedInformation provided by Micropol Limited
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
ISO 868
Tensile Strength, Yield 26.0 MPa
3770 psi
50mm/min; ISO 527-2
Elongation at Yield 7.0 %
7.0 %
50mm/min; ISO 527-2
Flexural Modulus 0.178 GPa
25.8 ksi
2mm/min; ISO 178
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
ISO 75-2