Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Minelco UltraCarb LH3 Hydrated Magnesium Calcium Carbonate

Category Ceramic , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Minelco Inc.
Trade Name UltraCarb
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Minelco UltraCarb LH3 Hydrated Magnesium Calcium Carbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mineral Flame RetardantUltracarb combines properties normally associated with several different materials that can be used jointly or individually to benefit many applications including rubber, plastics, surface coatings, mastics and sealants. The flame-retardant properties make it a valuable alternative to many of the traditional flame-retardants used in the plastics and rubber industry. The endothermic decomposition absorbs heat and reduces the flame and surface temperature of the burning polymer. The evolution of 53% of the original weight as non-flammable carbon dioxide and water vapor dilutes the oxygen near the burning surface as well as any smoke and flammable gases which are evolved during combustion.The onset of decomposition occurs at 220°C, allowing Ultracarb to be incorporated in high-melt polymers and enables improved compounding rates in intermediate melting point polymers. The fine particle size distribution of Ultracarb yields polymer compounds with good surface finish and improved mechanical properties.The product also offers rheological properties beneficial to the manufacture and practical application of a range of adhesives and sealants, providing a viable alternative to the precipitated calcium carbonates traditionally employed in these systems. In addition to flame retardant and rheological properties, Ultracarb offers a high brightness and neutral whiteness that makes it an ideal extender for titanium dioxide particularly in surface coating applications. Applications: Non-Halogen, Elastomers, Thermoset
Physical Properties Metric English Comments
Specific Gravity 2.50 g/cc
2.50 g/cc
Bulk Density 0.200 - 0.500 g/cc
0.00723 - 0.0181 lb/in³
Loose
Oil Absorption 20 - 40 %
20 - 40 %
Particle Size 0.50 µm
0.50 µm
10%
1.7 µm
1.7 µm
50%
6.0 µm
6.0 µm
90%
Specific Surface Area 17 m²/g
17 m²/g
Mechanical Properties Metric English Comments
Hardness, Mohs 2.5
2.5
Optical Properties Metric English Comments
Refractive Index 1.56
1.56
Component Elements Properties Metric English Comments
Al2O3 0.10 %
0.10 %
CaO 6.0 - 9.0 %
6.0 - 9.0 %
Fe2O3 0.050 %
0.050 %
K2O 0.010 %
0.010 %
Loss on Ignition(%) 51 - 54 %
51 - 54 %
MgO 36 - 39 %
36 - 39 %
SiO2 0.20 - 1.0 %
0.20 - 1.0 %
Sulfur, S 0.10 %
0.10 %
Descriptive Properties Value Comments
Acid Insoluble Matter, wt% 1 to 3
Appearance White powder
color (L*) 97
Moisture loss % 0.6
105°C