Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Momentive Performance Materials BIN77 Aluminum Nitride/ Boron Nitride Composite

Category Ceramic , Ceramic Matrix Composite , Nitride
Manufacturer Momentive Performance Materials (Former GE Advanced Ceramics)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials BIN77 Aluminum Nitride/ Boron Nitride Composite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Boron Nitride is a unique engineering material. It is a soft, machinable ceramic which can be combined with other refractory ceramics including Aluminum Oxide, Silicon Nitride, Aluminum Nitride, Mullite and Titanium Diboride. This results in composites which are machinable, thermal shock resistant, and chemically compatible in a wide range of environments. In combination with Titanium Diboride, for example, BN can be used as a heating source for the aluminum metallization of films and papers. BN composites are also used as break-rings in the horizontal continuous castings of steel and nozzles in rapid solidification processes. Other composite applications include the following: High temperature refractory shapesGlass forming tools and refractoriesMolds, dies and refractories for metalformingFurnace vents, stacks and fixturesInformation provided by Momentive Performance Materials, formerly GE Advanced Ceramics.
Physical Properties Metric English Comments
Density 2.43 g/cc
0.0878 lb/in³
Mechanical Properties Metric English Comments
Modulus of Elasticity 27.6 - 62.1 GPa
4000 - 9000 ksi
Sonic Modulus
Flexural Strength 124 MPa
18000 psi
27.6 MPa

@Temperature 1500 °C
4000 psi

@Temperature 2730 °F
Thermal Properties Metric English Comments
CTE, linear 5.00 - 6.00 µm/m-°C

@Temperature 20.0 °C
2.78 - 3.33 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 25.0 - 40.0 W/m-K
174 - 278 BTU-in/hr-ft²-°F