Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 25.0 W/m-K | 174 BTU-in/hr-ft²-°F | RT |
Outokumpu 4016 Ferritic Stainless Steel Fairly good corrosion resistant formable steel in mildly corrosive environments. Oxidation resistant at elevated temperatures (up to ~800°C). Ductile, does not work harden readily, and is well su.. |
|||
Thermal Conductivity | 25.0 W/m-K @Temperature 400 °C |
174 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Outokumpu 4016 Ferritic Stainless Steel Fairly good corrosion resistant formable steel in mildly corrosive environments. Oxidation resistant at elevated temperatures (up to ~800°C). Ductile, does not work harden readily, and is well su.. |
|||
Thermal Conductivity | 25.0 W/m-K @Temperature 400 °C |
174 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Outokumpu 4021 Martensitic Stainless Steel Moderate corrosion resistant stainless steel hardenable up to 1000N/mm2. Re-sulphurized steel improves machining properties.Applications: ShaftsKnivesFastenersSurgical applicationsDomestic applicat.. |
|||
Thermal Conductivity | 25.0 W/m-K @Temperature 400 °C |
174 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Outokumpu 4028 Martensitic Stainless Steel Moderate corrosion resistant stainless steel hardenable up to 1000N/mm2. Re-sulphurized steel improves machining properties.Applications: ShaftsKnivesFastenersSurgical applicationsDomestic applicat.. |
|||
Thermal Conductivity | 25.0 W/m-K @Temperature 85.0 °C |
174 BTU-in/hr-ft²-°F @Temperature 185 °F |
|
Indium Corp. Indalloy 155 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Thermal Conductivity | 25.0 W/m-K @Temperature 85.0 °C |
174 BTU-in/hr-ft²-°F @Temperature 185 °F |
|
Indium Corp. Indalloy® 164 Pb-In-Ag Solder Alloy This alloy is very useful in the 300°C range. It has particularly good thermal fatigue properties as well as the minimal gold leaching properties of indium-lead alloys. Often used in reducing atm.. |
|||
Thermal Conductivity | 25.0 - 40.0 W/m-K | 174 - 278 BTU-in/hr-ft²-°F | |
Momentive Performance Materials BIN77 Aluminum Nitride/ Boron Nitride Composite Boron Nitride is a unique engineering material. It is a soft, machinable ceramic which can be combined with other refractory ceramics including Aluminum Oxide, Silicon Nitride, Aluminum Nitride, Mu.. |
|||
Thermal Conductivity | 25.0 W/m-K @Temperature 100 °C |
174 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Latrobe Lescalloy® 410Cb High Strength Stainless Steel LESCALLOY 17-4 VAC-ARC steel is a precipitation hardening martensitic stainless steel. A wide range of mechanical properties is available via simple aging within a 900-1150°F (482-621°C) tempe.. |
|||
Thermal Conductivity | 25.0 W/m-K @Temperature 85.0 °C |
174 BTU-in/hr-ft²-°F @Temperature 185 °F |
|
Indium Corp. Indalloy 12 Lead Solder Alloy Tin-free indium solderInformation Provided by Indium Corporation |
|||
Thermal Conductivity | 25.0 W/m-K @Temperature 85.0 °C |
174 BTU-in/hr-ft²-°F @Temperature 185 °F |
|
Indium Corp. Indalloy® 159 Pb-Sn Solder Alloy High temp solder for BGA applications.Information provided by the manufacturer, Indium Corporation. |
|||
Thermal Conductivity | 25.0 W/m-K @Temperature 20.0 °C |
174 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Industeel SOLEIL A2 13% Cr High Strength Martensitic Stainless Steel (QT550 Heat Treatment) Description: Soleil A2 has combined Chromium (~13%) and Carbon ~0.10%) additions to provide an excellent combination of high mechanical properties and improved corrosion resistance properties. The g.. |
|||
Thermal Conductivity | 25.0 W/m-K | 174 BTU-in/hr-ft²-°F | |
Specialty Materials Boron Monofilament Exceptional compression strength. Specialty Materials' Chemical Vapor Deposition process uses fine tungsten wire for the substrate and boron trichloride gas as the boron source.Information prov.. |
|||
Thermal Conductivity | 25.0 W/m-K | 174 BTU-in/hr-ft²-°F | |
Sapco 98% Aluminum Oxide Information provided by Sapco. |
|||
Thermal Conductivity | 25.0 W/m-K | 174 BTU-in/hr-ft²-°F | |
Williams Advanced Alloys WS300 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Thermal Conductivity | 25.0 W/m-K | 174 BTU-in/hr-ft²-°F | |
CoorsTek StatSafe™ ADC Static Dissipative Alumina Specialized StatSafe™ ESD-safe alumina combines static-dissipation characteristics with the mechanical properties of advanced ceramics: tailorable volume resistivity, surface finish, high stiffnes.. |
|||
Thermal Conductivity | 25.0 W/m-K | 174 BTU-in/hr-ft²-°F | |
China-Yixing Longly Refractories ZTA (10%ZrO2) Zirconia Toughened Alumina Composite Ceramic LONGLY's Zirconia Toughened Alumina ceramics (hereafter referred as composite ceramic, ZTA) is white, corrosion resistance, good chemical stability. As well all know that alumina is hard, while zir.. |
|||
Thermal Conductivity | 25.0 W/m-K | 174 BTU-in/hr-ft²-°F | 409 HP™ |
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 14% Cold Work AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze.. |
|||
Thermal Conductivity | 25.0 W/m-K | 174 BTU-in/hr-ft²-°F | 409 HP™ |
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 2.9% Cold Work AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze.. |
|||
Thermal Conductivity | 25.0 W/m-K | 174 BTU-in/hr-ft²-°F | 409 HP™ |
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 43.6% Cold Work AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze.. |
|||
Thermal Conductivity | 25.0 W/m-K | 174 BTU-in/hr-ft²-°F | 409 HP™ |
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 8.5% Cold Work AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze.. |
|||
Thermal Conductivity | 25.0 W/m-K | 174 BTU-in/hr-ft²-°F | |
ATI Allegheny Ludlum AL 409HP™ Ferritic Stainless Steel, UNS S40930 Type 409 ferritic stainless steel was introduced by Allegheny Ludlum in 1961 to provide improved oxidation and corrosion resistance for automotive exhaust systems in comparison to carbon automotive .. |
|||
Thermal Conductivity | 25.0 W/m-K | 174 BTU-in/hr-ft²-°F | 409 HP™ |
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel, 20% Cold Work AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze.. |
|||
Thermal Conductivity | 25.0 W/m-K @Temperature 20.0 - 100 °C |
174 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
Anderman Ceramics EA995 Sintered Alumina, 99.5% Densely sintered alumina is characterized by: high strength and hardness, temperature stability, electrical insulation, and high wear resistance and corrosion resistance even at high temperatures. .. |
|||
Thermal Conductivity | 25.0 W/m-K | 174 BTU-in/hr-ft²-°F | |
Ceradyne Ceralloy® 225 Titanium Diboride Features:electrical conductancewear resistancehardnessApplications:wear componentsballistic armorsputtering targetsInformation provided by Ceradyne Company |
|||
Thermal Conductivity | 25.0 W/m-K | 174 BTU-in/hr-ft²-°F | 409 HP™ |
ATI Allegheny Ludlum AL 409 Cb™ Brazeable Ferritic Stainless Steel AL 409 Cb™ is normally 12.5% chromium ferritic stainless steel with columbium stabilization and with restricted titanium and aluminum contents. As a result of these alloying adjustments, the braze.. |
|||
Thermal Conductivity | 25.0 W/m-K | 174 BTU-in/hr-ft²-°F | |
Industeel Superplast® Stainless Mold Steel SUPERPLAST® Stainless is a specially designed steel for plastic mould bases providing improved performances compared to standard grades such as 1.2085. SUPERPLAST® Stainless offers improved machi.. |
|||
Thermal Conductivity | >= 25.0 W/m-K | >= 174 BTU-in/hr-ft²-°F | |
Advanced Ceramics ACL 1091 (C-799) Alumina Information provided by Advanced Ceramics Limited (ACL) |
|||
Thermal Conductivity | 25.0 W/m-K @Temperature 20.0 °C |
174 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Industeel SOLEIL A2 13% Cr High Strength Martensitic Stainless Steel (QT650 Heat Treatment) Description: Soleil A2 has combined Chromium (~13%) and Carbon ~0.10%) additions to provide an excellent combination of high mechanical properties and improved corrosion resistance properties. The g.. |