Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Momentive Performance Materials HCPH Boron Nitride (BN) Powder

Category Ceramic , Nitride , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Momentive Performance Materials (Former GE Advanced Ceramics)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials HCPH Boron Nitride (BN) Powder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
GE Advanced Ceramics boron nitride (BN) powders of grades HCP, HCPH, HCPL, and AC6004 are generally single-crystal hexagonal platelets with very high purity. The mean particle sizes for these ultra-fine powders are in the range of 6 to 13 µm, and they are >99.9% -325 mesh.HCPH is processed to consist of a more agglomerated structure than HCP, and therefore a higher specific surface area. This makes it ideal for creating good particle-to-particle contact in a matrix.Information provided by Momentive Performance Materials, formerly GE Advanced Ceramics.
Physical Properties Metric English Comments
Bulk Density 0.350 g/cc
0.0126 lb/in³
Tap Density
Particle Size 3.0 µm
3.0 µm
Crystal Size
6.0 - 9.0 µm
6.0 - 9.0 µm
Mean
Specific Surface Area 17 m²/g
17 m²/g
Descriptive Properties Value Comments
Carbon 0.03%
Color White
Crystal Type Hexagonal (Graphitic)
Oxygen 0.5%
Sol. Borate 0.2%