Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Momentive Performance Materials PolarTherm® PT100 Boron Nitride (BN) Powder

Category Ceramic , Nitride , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Momentive Performance Materials (Former GE Advanced Ceramics)
Trade Name PolarTherm®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials PolarTherm® PT100 Boron Nitride (BN) Powder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Single crystal platelet BN Powder. High aspect ratio platelets may improve thermal conductivity when used as a filler in polymers or lubricants. Features of BN include thermal conductor, electrical insulator, low dielectric constant, high temperature stability, lubricious, inert, and non-wetting.Information provided by Momentive Performance Materials.
Physical Properties Metric English Comments
Bulk Density 0.270 g/cc
0.00975 lb/in³
Tap Density
Particle Size >= 7.0 µm
>= 7.0 µm
D10
13 µm
13 µm
Mean
<= 25 µm
<= 25 µm
D90
Specific Surface Area 5.5 m²/g
5.5 m²/g
Descriptive Properties Value Comments
Carbon 0.05%
Morphology Hexagonal
Oxygen 0.2%
Sol. Borate 0.1%
Users viewing this material also viewed the following: