Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 5.5 m²/g | 5.5 m²/g | |
Omya OMYACARB® FT - FL Calcium Carbonate A high purity, fine, wet ground, surface-treated natural calcium carbonate.Applications: Plastic applications such as rigid PVC and flexible PVC. Paint applications such as water based, solvent base.. |
|||
Specific Surface Area | 5.5 m²/g | 5.5 m²/g | |
Omya OMYACARB® FT HS-FL Calcium Carbonate A high purity, fine, wet ground, surface-treated natural calcium carbonate.Applications: Plastic applications such as rigid PVC and flexible PVC. Paint applications in solvent based and powder coati.. |
|||
Specific Surface Area | 5.5 m²/g | 5.5 m²/g | |
PPT LSF120 Low Sintering Temperature Ferrite Powder Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4.. |
|||
Specific Surface Area | 5.5 m²/g | 5.5 m²/g | |
PPT LSF16 Low Sintering Temperature Ferrite Powder Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4.. |
|||
Specific Surface Area | 5.5 m²/g | 5.5 m²/g | |
PPT LSF180 Low Sintering Temperature Ferrite Powder Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4.. |
|||
Specific Surface Area | 5.5 m²/g | 5.5 m²/g | |
PPT LSF220 Low Sintering Temperature Ferrite Powder Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4.. |
|||
Specific Surface Area | 5.5 m²/g | 5.5 m²/g | |
PPT LSF25 Low Sintering Temperature Ferrite Powder Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4.. |
|||
Specific Surface Area | 5.5 m²/g | 5.5 m²/g | |
PPT LSF400 Low Sintering Temperature Ferrite Powder Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4.. |
|||
Specific Surface Area | 5.5 m²/g | 5.5 m²/g | |
PPT LSF50 Low Sintering Temperature Ferrite Powder Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4.. |
|||
Specific Surface Area | 5.5 m²/g | 5.5 m²/g | |
Momentive Performance Materials PolarTherm® PT100 Boron Nitride (BN) Powder Single crystal platelet BN Powder. High aspect ratio platelets may improve thermal conductivity when used as a filler in polymers or lubricants. Features of BN include thermal conductor, electrica.. |