Multibase Multi-ABS 802 Utility Grade White

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer Multibase
Trade Name Multi-ABS
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-ABS 802 Utility Grade White.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792-91
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955-89
Melt Flow 3.0 g/10 min
3.0 g/10 min
(Condition I) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Shore D 103
103
10 sec; ASTM D-2240-95
Tensile Strength, Ultimate 33.1 MPa
4800 psi
ASTM D638-95
Elongation at Break 17 %
17 %
ASTM D638-95
Flexural Modulus 1.828 GPa
265.1 ksi
Method 1, Proc. B; ASTM D-790-95
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
ASTM D256-93a