Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Flex® D 5302 ELF Black TPO Thermoplastic Polyolefin Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Polyolefin
Manufacturer Multibase
Trade Name Multi-Flex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® D 5302 ELF Black TPO Thermoplastic Polyolefin Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 0.962 g/cc
0.962 g/cc
ASTM 792
Melt Flow 1.32 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.32 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 39
39
10 seconds; ASTM D2240
Tensile Strength, Yield 17.1 MPa
2480 psi
Elastic; ASTM D412
Elongation at Break 630 %
630 %
Elastic; ASTM D412
Flexural Modulus 0.214 GPa
31.0 ksi
ASTM D790
Tear Strength 91.2 kN/m
520 pli
ASTM D624
Users viewing this material also viewed the following: