Mechanical Properties Metric English Comments
Flexural Modulus 0.214 GPa
31.0 ksi
ISO 178/1A
Radici Heraflex® E 4718 TPC-ET Thermoplastic Elastomer
TPC-ET Thermoplastic Elastomer. Low Modulus, Nominal Shore D/15s 43. Natural colorProcessing technology: Injection moldingInformation provided by Radici group.
Flexural Modulus 0.214 GPa
31.0 ksi
1% secant; ASTM D790
ExxonMobil LD 051.LJ Molding, Extrusion and Compounding Resin  (discontinued **)
LD 051.LJ resin is used in Blow molded, squeeze bottles, Pail lids, Closures, and Extruded profiles.Information provided by ExxonMobil Chemical
Flexural Modulus 0.214 GPa
31.0 ksi
ASTM D790
Multibase Multi-Flex® D 4000 TPO Thermoplastic Polyolefin Elastomer
Forms: PelletsProcessing Methods:Blow MoldingInformation provided by Multibase
Flexural Modulus 0.214 GPa
31.0 ksi
ASTM D790
Multibase Multi-Flamâ„¢ 2903 LDPE Polyethylene
Features:Flame RetardantHalogen Content, Low to NoneBlooming, None Forms:PelletsProcessing Methods:Injection MoldingExtrusionCoextrusionUses:TubingPipingInformation provided by Multibase
Flexural Modulus 0.214 GPa
31.0 ksi
ASTM D790
Multibase Multi-Flex® D 5302 ELF Black TPO Thermoplastic Polyolefin Elastomer
Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Flexural Modulus 0.214 - 0.262 GPa
31.0 - 38.0 ksi
Average value: 0.236 GPa Grade Count:5
Overview of materials for Low Density Polyethylene (LDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi..
Flexural Modulus 0.214 GPa
31.0 ksi
ASTM D790
Amco PRIMATOP LDPE 023919 Blow Molding Polyethylene
LDPE 023919 features good heat sealing latitude and easy processability. Applications include food contact, squeeze bottles, and non-escr.Former A-Top Polymers product; part of Amco product line sin..
Flexural Modulus 0.214 GPa
31.0 ksi
ASTM D790
Chase Plastics CP Pryme® PE-100LD20M General Purpose Low Density Polyethylene
Information provided by Chase Plastics.
Copyright © lookpolymers.com All Rights Reserved