Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Flex® TPE A 7150 BLK

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Multibase
Trade Name Multi-Flex® TPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPE A 7150 BLK.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.83 g/cc
0.0661 lb/in³
ASTM D792
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955
Melt Flow 5.0 - 22 g/10 min
5.0 - 22 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 89
89
10 sec; ASTM D-2240
Tensile Strength, Ultimate >= 4.80 MPa
>= 696 psi
ASTM D412
Elongation at Break >= 400 %
>= 400 %
ASTM D412
Flexural Modulus 0.170 GPa
24.7 ksi
method 1, Proc.B; ASTM D-790
Tear Strength >= 30.0 kN/m
>= 171 pli
ASTM D624
Users viewing this material also viewed the following: