Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.83 g/cc | 0.0661 lb/in³ | ASTM D792 |
Multibase Multi-Flex® TPE A 7150 BLK The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Density | 1.83 g/cc | 0.0661 lb/in³ | ASTM D792 |
Plenco 50125 PET, Pellet, Injection Molded, White
(discontinued **) PLENCO 50125 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in white only.Inform.. |
|||
Density | 1.83 g/cc | 0.0661 lb/in³ | ASTM D792 |
Rogers Corporation RO4450F Prepreg Prepreg is commonly used to inexpensively form less critical signal layers in antenna designs. A high post-cure Tg makes RO4400 series prepreg an excellent choice for multi-layers requiring sequent.. |
|||
Density | 1.83 g/cc | 0.0661 lb/in³ | Crystalline; ISO 1183 |
Victrex® PEEK 90GL60 Polyetheretherketone, 60% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 60% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, standard flow, FDA food contac.. |
|||
Density | 1.83 g/cc | 0.0661 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Solef® 3108/0903 Anti-static PVDF Compound
(discontinued **) Key features of this grade: Anti-static, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crystall.. |
|||
Density | 1.83 g/cc | 0.0661 lb/in³ | |
IDI Composites 44-10 HGM Thermoset Polyester, Molding Same as 44-10 HG with Mil Spec MAI-60.Data provided by the manufacturer. |
|||
Density | 1.83 g/cc | 0.0661 lb/in³ | ASTM D572 |
Haysite ETR-FR-C Glass Reinforced Polyester Sheet, Electrical Grade (GPO3) ETR-FR-C meets NEMA GPO-3 requirements and exceeds NEMA in dielectric strength, arc resistance, and track resistance. This U.L. recognized grade is highly flame retardant and low smoke generating. E.. |
|||
Density | 1.83 g/cc | 0.0661 lb/in³ | ASTM D572 |
Haysite H-193 Corrosion Resistant Polyester/Glass Sheet A fiber glass reinforced thermoset polyester sheet having good corrosion resistance to numerous acids and alkalis. This material also exhibits a high level of flame retardancy and low smoke generati.. |
|||
Density | 1.83 g/cc | 0.0661 lb/in³ | ASTM D792 |
Glastic Laminates/Shapes 1580 Polyester Laminate Data provided by Glastic Corporation.NEMA GPO-3. Developed to meet the television industry's safety assurance requirements. |
|||
Density | 1.83 g/cc | 0.0661 lb/in³ | ASTM D891 |
Solvay Specialty Polymers FOMBLIN® LC08 PFPE Lubricant FOMBLIN LC perfluoropolyether fluids have the following unique features: excellent wear characteristics; very good low temperature properties; cost-effective; and outstanding for applications requir.. |
|||
Density | 1.83 g/cc | 0.0661 lb/in³ | ASTM D891 |
Solvay Specialty Polymers FOMBLIN® M15 PFPE Lubricant Information provided by Solvay Solexis, Inc. |
|||
Density | 1.83 g/cc @Temperature 25.0 °C |
0.0661 lb/in³ @Temperature 77.0 °F |
|
Solvay Specialty Polymers Galden® HS260 PFPE VPS Fluid Galden® LS and HS grades are specifically recommended for vapor phase soldering.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of servic.. |
|||
Density | 1.83 g/cc | 0.0661 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP 2Z004 ETFE LNP* THERMOCOMP* 2Z004 is a compound based on ETFE resin containing 20% Milled Glass. |
|||
Density | 1.83 g/cc | 0.0661 lb/in³ | Relative Density; ASTM D792 |
Sumitomo Bakelite North America RX® 1-520/RX® 1310 Short-Glass Reinforced Diallyl Phthalate Short glass fiber reinforced, non-flame retardant, diallyl ortho-phthalate molding compound which meets the requirements of ASTM D5948 Type SDG.Information provided by Vyncolit, a Sumitomo Bak Group.. |
|||
Density | 1.83 g/cc | 0.0661 lb/in³ | Relative Density; ASTM D792 |
Sumitomo Bakelite North America RX® 3-1-501N-P Mineral Filled Diallyl Phthalate Mineral filled, flame retardant, diallyl ortho-phthalate molding compound which meets the requirements of ASTM D5948 Type MDG-F.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Density | 1.83 g/cc | 0.0661 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp 2Z004 FP-E (EFTE) LNP* 2Z004 is a compound based on Ethylenetetrafluoroethylene (ETFE) containing Milled Glass.This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.83 g/cc | 0.0661 lb/in³ | ASTM D792 |
Plenco 05118-T5 Phenolic, Granular, Compression Molded PLENCO 05118-T5 is a mineral and graphite filled novolac phenolic molding compound with PTFE, formulated for bearing seals. 05118 provides for a low coefficient of friction, good wear resistance, ve.. |
|||
Density | 1.83 g/cc | 0.0661 lb/in³ | ASTM D792 |
Plenco 08218 Polyester BMC, Compression Molded PLENCO 08218 is a renumber of PlasGlas 20118. PLENCO 08218 is an 18% glass-filled polyester bulk molding compound characterized as an electrical grade, but has many outstanding properties that make .. |
|||
Density | 1.83 g/cc | 0.0661 lb/in³ | ASTM D792 |
Plenco 1581 Polyester, Pellet, Injection Molded PLENCO 01581 is a glass and mineral reinforced pelletized polyester molding compound, exhibiting excellent dimensional stability, mechanical strength and also arc resistance, track resistance, and f.. |
|||
Density | 1.83 g/cc | 0.0661 lb/in³ | ASTM D792 |
Plenco 7556 Phenolic, Briquette, Transfer Molded PLENCO 07556 is a glass fiber reinforced novolac phenolic molding compound, with good physical strengths and heat resistance along with excellent dimensional stability. UL recognized under component.. |
|||
Density | 1.83 g/cc | 0.0661 lb/in³ | ISO 1183 |
DuPont Performance Polymers Rynite® FR531 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 36% Reinforced Flame Retardant Polyethylene Terephthalate Information provided by DuPont Performance Polymers |
|||
Density | 1.83 g/cc | 0.0661 lb/in³ | ISO 1183 |
Eurotec® Tecopet® PT70 KK45 PET, 45% glass fiber/mineral reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Density | 1.83 g/cc | 0.0661 lb/in³ | ASTM D792 |
Applied Composites 8068 Polyester SMC Industry Application: High StrengthProduct Application: MilitaryDistinct Features: Structural Grade Chopped and Unidirectional Fibers, High Stiffness, High Fiber LoadingsInformation provided by Appl.. |
|||
Density | 1.83 - 2.03 g/cc | 0.0661 - 0.0733 lb/in³ | Molded |
Bulk Molding Compounds BMC T14 General Purpose Molding Compound BMC T14 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T14 is well suited for injection, transfer or compression molding of intricate parts. Typica.. |
|||
Density | 1.83 - 2.03 g/cc | 0.0661 - 0.0733 lb/in³ | Molded |
Bulk Molding Compounds BMC T15(GP) General Purpose Molding Compound BMC T15(GP) is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15(GP) is well suited for a variety of applications. It is av.. |
|||
Density | 1.83 - 2.03 g/cc | 0.0661 - 0.0733 lb/in³ | Molded |
Bulk Molding Compounds BMC A50-MS General Purpose Molding Compound BMC A50-MS is a medium strength, high appearance, general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC A50-MS is well suited for injection, transfer or compres.. |
|||
Density | 1.83 g/cc | 0.0661 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP WX05502 Polyester, TP (Asia Pacific) LNP* THERMOCOMP* WX05502 is a compound based on Polyester, TP resin containing Flame Retardant, Mineral, Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Density | 1.83 g/cc | 0.0661 lb/in³ | ASTM D792 |
Plenco 1581 Polyester, Briquette, Transfer Molded PLENCO 01581 is a glass and mineral reinforced pelletized polyester molding compound, exhibiting excellent dimensional stability, mechanical strength and also arc resistance, track resistance, and f.. |
|||
Density | 1.83 g/cc | 0.0661 lb/in³ | ASTM D-792 |
Sumitomo Bakelite North America FM 4005X4649 Fiberglass Reinforced Phenolic Novolac FM 4005X4649 a fiberglass reinforced two-step phenolic molding compound formulated to increase thermal conductivity, to provide static dissipation and good wear resistance to abrasive media.Informat.. |