Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Flex® TPE A 8502 P BLK , 37.5% Filler Content

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Multibase
Trade Name Multi-Flex® TPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPE A 8502 P BLK , 37.5% Filler Content.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The following data represents the actual data obtained from Lot # 941101-5. The moisture content is 0.03%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.998 g/cc
0.0361 lb/in³
ASTM D792
Melt Flow 15 g/10 min
15 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 92
92
10 sec; ASTM D-2240
Tensile Strength, Ultimate 9.70 MPa
1410 psi
ASTM D638
Elongation at Break 635 %
635 %
ASTM D638
Tear Strength 50.7 kN/m
289 pli
ASTM D624
Users viewing this material also viewed the following: