Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.998 g/cc | 0.0361 lb/in³ | ASTM D792 |
Multibase Multi-Flex® TPE A 8502 P BLK , 37.5% Filler Content The following data represents the actual data obtained from Lot # 941101-5. The moisture content is 0.03%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Density | 0.998 g/cc | 0.0361 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON MD000A PP LNP* STAT-KON* MD000A is a compound based on Polypropylene resin containing Carbon. Added feature of this grade is: Electrically Conductive. |
|||
Density | 0.998 g/cc | 0.0361 lb/in³ | indicative |
Solvay CATAFOR® F Surfactant Identification: QUATERNARY AMMONIUM ETHOSULPHATECAS: 68308 – 64 – 5Solubility: Soluble in water. Soluble in organic polar solvents.Solvent: Ethylene glycol 20%Available in: Asia Pacific, .. |
|||
Density | 0.998 g/cc | 0.0361 lb/in³ | |
BASF D 2000 Polyetheramine Formula: C5H9ClOCAS: 9046-10-0Description Polyetheramine D 2000 is a yellowish liquid, with an amine-like odor. It is partly miscible with water and other solvents. Synonyms: Polyetheramine D2000, .. |
|||
Density | 0.998 g/cc | 0.0361 lb/in³ | |
BASF N-Ethylpyrrolidone-2 (NEP) Formula: C6H11NOCAS: 2687-91-4Description: N-Ethylpyrrolidone-2 (NEP) Is a colorless to yellow liquid, with an amine like odor. It is miscible in water and soluble in other organic solvents.Synonym.. |